How To Prevent Feed Pellet Machine Failures?
Leave a message
During the production of the pellet machine, if the pellets have axial cracks or radial cracks, and the powdering rate is high and the output is low, the reason for this phenomenon may be that the quenching and tempering temperature cannot be reached and the material is poorly matured. Increase the quenching and tempering temperature and increase the amount of steam during quenching and tempering; it may also be that the cutter is far away and blunt, causing the particles to be shortened or torn instead of cut; the surface of the particles is not very smooth, and the powdering rate is high, which may The ring die compression ratio is small, and the compression hole should be enlarged. Ring die compression; the particle surface is smooth, but the hardness is too high. It may be that the ring die compression ratio is large, and the ring die compression ratio should be reduced.

| Model | Capacity (kg/hr) | Power(KW) | Weight(kg) | Dimension (cm) |
| MK-125 | 80-100 | 3 | 95 | 110*35*700 |
| MK-150 | 110-150 | 4 | 98 | 115*35*80 |
| MK-210 | 200-300 | 7.5 | 280 | 115*45*95 |
| MK-230 | 350-450 | 11 | 300 | 138*46*100 |
| MK-260 | 500-600 | 15 | 315 | 130*53*105 |
| MK-300 | 700-800 | 22 | 600 | 145*62*120 |
| MK-360 | 800-900 | 22 | 795 | 160*67*145 |
| MK-400 | 1000-1200 | 30 | 1000 | 160*67*145 |
When the particle moisture content is high, the production output is low, and machine blockage often occurs. It may be that the pressure reducing valve cannot reduce pressure or the drain valve cannot drain water. The pressure reducing valve should be adjusted to increase the steam pressure entering the conditioner. It is 0.1-0.4MPa, and enables the trap to play a hydrophobic role. The quenching and tempering temperature can also be increased accordingly, because an increase in temperature is conducive to the improvement of the maturation degree of the material. Generally, the moisture content of the material increases by about 1% for every 11°C increase in temperature. Pellets are of different lengths, so the cutter distance or material distribution should be adjusted. Deflection scraper position; where the current deviation between the two motors is large, the tension of the belts of the two motors should be adjusted to make the tension as consistent as possible.