Home - Knowledge - Details

Why a Floating Fish Feed Extruder Sprays Material and How to Fix It

Material Spraying Starts at the Screw and Barrel

On a floating fish feed extruder, raw material that sprays back out of the feed inlet is almost always a conveying problem inside the machine, not a problem with the formula. The screw grips the mash and pushes it forward; the barrel surrounds the screw and keeps the material in the compression zone. When the screw cannot grip, or the barrel cannot hold the material, feed backs up at the inlet and is thrown out. Many operators change the recipe first, but checking screw and barrel condition identifies the real cause in a few minutes.

The faults divide neatly into two groups. Screw faults are loss of thread depth and loss of concentricity. Barrel faults are damage to the inner wall and loss of heating in one section. Each has a measurable check and a defined repair.

Screw Faults That Cause Spraying

Severe thread wear

The flight on the screw grips the material, and its depth decides how much material is carried into the compression zone. Over a long production period the edges round off and the thread flattens; a flight that started 5 mm deep can wear down to about 2 mm. Carry capacity falls, material collects at the inlet and sprays out.

Remove the screw and measure the remaining thread depth with a depth gauge or caliper.

If wear exceeds roughly one third of the original depth, replace the screw with a new one of the same diameter as the barrel, for example a 65 mm screw for a 65 mm barrel.

If wear is light, dress the thread edges with fine abrasive paper and restore a clean gripping edge; monitor output per hour afterwards to confirm recovery.

Screw misalignment

If the screw axis is not concentric with the barrel bore, one side runs almost flush against the barrel wall while a gap opens on the opposite side. Material leaks back through the gap, accumulates at the inlet and sprays out, and the machine also runs with a distinctive rubbing noise.

Stop the machine, isolate the power and disassemble the extruder head.

Reinstall the screw and check the axis with a dial indicator or a level along the screw length.

Tighten the fixing bolts progressively and turn the screw by hand; it should rotate freely with no tight spot and no axial play.

Barrel Faults That Cause Spraying

Scratches and dents on the inner wall

Metal fragments, hard grit and long service at high temperature and pressure can score the barrel bore. Material lodges in the grooves, cannot be carried forward, and the material behind it is pushed back out of the inlet.

Inspect the bore under light along its full length after each screw removal.

Light scratches can be smoothed with fine abrasive paper of 200 grit or finer, working circumferentially and keeping the bore round.

Deep scratches or pronounced dents mean the barrel must be replaced; running a damaged barrel accelerates screw wear and makes the spraying worse.

Uneven heating between sections

The barrel is heated in sections, commonly three. Each section has its own heating element and set point. If one element fails, that section never reaches its set temperature; a section set to 120 degrees C may only reach 80 degrees C. Material entering the cold section does not soften or expand, it stalls and builds up pressure until it sprays from the inlet.

Measure each section with a contact thermometer or infrared thermometer during a warm-up cycle.

Locate the failed element and replace it with an element of the same power rating, for example a 2 kW element replaced by another 2 kW element.

Allow a full warm-up and confirm that every section is within its tolerance band before feeding material.

Inspection Before and During Production

Before every startup, turn the screw by hand through several revolutions; a screw that binds by hand will certainly fail under load.

Listen to the barrel once material is flowing. Squeaking or grinding points to screw or barrel damage and is a reason to stop immediately rather than finish the batch.

Record inlet temperature, section temperatures, screw speed and extrusion current each shift so that a drifting section is spotted before it becomes a blockage.

Keep the die and cutter clean and check that the extruder head bolts are evenly tightened, because a loose head on one side also opens a path for material to escape.

Four Misconceptions About Material Spraying

Spraying means the raw material is unsuitable. Screw and barrel condition should always be inspected first, since the same formula runs correctly on a sound machine.

Light thread wear can wait until the machine stops. Output per hour and pellet quality fall long before the extruder stops completely.

Any spare heating element will do. Fitting an element of a different power changes the temperature balance of the whole barrel and can cause a new blockage elsewhere.

Running on after a grinding sound is harmless. Stopping at once is what protects the screw and barrel from permanent scoring.

Frequently Asked Questions

Q: Why does material spray from the inlet instead of the die?
Because the screw can no longer move material forward. Thread wear, misalignment, a scored barrel or a cold barrel section all reduce forward conveying, and the mash takes the path of least resistance back out of the inlet.

Q: How much thread wear is acceptable before replacement?
Measure the remaining depth against the original figure. Wear beyond about one third of the original depth means the screw cannot grip reliably and should be replaced rather than dressed.

Q: Can a wrong heating element cause spraying?
Yes. A lower-power element leaves its section cold, so material stalls there and backs up. Always fit a replacement with the same power rating as the original.

Q: How do I check screw alignment after reassembly?
Turn the screw by hand after tightening the fixing bolts. It should rotate smoothly along the full length with no tight point; if it binds, recheck the axis with a level or dial indicator before running the machine.

Q: How often should the barrel bore be inspected?
Inspect it every time the screw is removed for maintenance, and at least once per production season, using a bright lamp along the bore to reveal scoring and material build-up.

Q: Does the die affect spraying as well?
A partly blocked die raises back pressure in the compression zone, which amplifies any existing screw or barrel problem. Keep the die openings clear and the head bolts evenly tightened.

Send Inquiry